Knowledge

Measuring which anodes are copper, aluminium or iron

To tell whether an anode is a copper anode (anti-fouling) or a corrosion-protection anode (aluminium or iron), measure the potential from the anode to ground. For the reading to be valid, the anode must not have had voltage applied for a day or more. An anode in seawater produces a potential, much like a battery, because of the potential difference relative to steel. See the table below. These are potential readings in millivolts.

Potential table

A/F or A/C anodeNo sacrificial anodesSacrificial anodes in seachests
MSZnAl
Cu (copper)250–400 (+)650–900 (+)600–850 (+)
Al (aluminium)100–250 (−)100–200 (+)0
Fe (iron)0–150 (+)300–400 (+)200–400 (+)

Values are in millivolts (mV). MS = mild steel, Zn = zinc, Al = aluminium.

From the Cathelco manual

The table above shows the expected range in millivolts of the potential between anode and ground. If there are sacrificial anodes in the sea chest, or even near it on the shell, the last two columns will apply; otherwise the first will show the upper range of expected values. In the absence of sacrificial anodes in the sea chest, the better the paint job and cathodic protection of the outer hull, the nearer the value will be to the right hand figure in the first column of the table. Very low potential difference is likely to indicate loss of continuity or breakdown of insulation of the circuit, except in the cases where anode and hull or sacrificial materials are the same, or very close in the galvanic series. Potential readings are also useful for verifying that anti-fouling and corrosion suppression cables have not been crossed over, which is important where different currents are specified.